Japanese Standard (JIS)
Chemical composition, Mechanical properties and weld test properties of tube according to standards.
STANDARD | TYPE | CHEMICAL COMPOSITION | MECHANICAL PROPERTIES | WELD TEST PROPERTIES | |||||||||||
C% | Mn% | So/o | P% | Si% | YS KG/SQ MM | TS KG/SQ MM | %EL Min | FLARING % | Flattening @90 Deg | Flattening @180 Deg | Bending | Crushing | Flanging | ||
JIS 3445/1983 | STKM-1lA | 0.12 max | 0.60 max | 0.04 max | 0.04 max | 0.35 max | - | 30 | 35 | - | 1/2 D | 1/2 D | 180°/40 | - | - |
STKM-12A | 0.20 max | 0.60 max | 0.04 max | 0.04 max | 0.35 max | 18 | 35 | 35 | - | 2/3 D | 2/3 D | 90°/60 | - | - | |
STKM-12B | 0.20 max | 0.60 max | 0.04 max | 0.04 max | 0.35 max | 28 | 40 | 25 | - | 2/3 D | 2/3 D | 90°/60 | - | - | |
STKM-12C | 0.20 max | 0.60 max | 0.04 max | 0.04 max | 0.35 max | 36 | 48 | 20 | - | - | - | - | - | - | |
STKM-13A | 0.25 max | 0.30 max | 0.04 max | 0.04 max | 0.35 max | 22 | 38 | 30 | - | 2/3 D | 2/3 D | 90°/60 | - | - | |
STKM-13B | 0.25 max | 0.30 max | 0.04 max | 0.04 max | 0.35 max | 31 | 45 | 20 | - | 3/4 D | 3/40 | 90°/60 | - | - | |
STKM-13C | 0.25 max | 0.30 max | 0.04 max | 0.04 max | 0.35 max | 39 | 52 | 15 | - | - | - | - | - | - | |
JIS 4361/1948 | STB-35 | 0.18 max | 0.30 max | 0.35 max | 0.35 max | 0.35 max | 18 | 35 | 30 | 20 | 3t | - | - | - | - |
STB-42 | 0.32 max | 0.30 max | 0.35 max | 0.35 max | 0.35 max | 26 | 42 | 30 | 20 | 3t | - | - | - | - | |
JIS 3466/1982 | SKTMR-42 | 0.25 max | 0.30 max | 0.04 max | 0.04 max | - | 25 | 41 | 23 | - | - | - | - | - | - |
SKTMR-50 | 0.18 max | 1.50 max | 0.04 max | 0.04 max | 0.55 max | 33 | so | 23 | - | - | - | - | - | - |